pone.0239034.g001.tif (207.37 kB)

Thermal decomposition of Mn(II) ACAC was performed in oleylamine and dibenzyl ether at two temperature ramp rates and increasing aging times at 300°C to form MnO NPs coated with oleylamine.

Download (207.37 kB)
figure
posted on 18.09.2020 by Celia Martinez de la Torre, Jasmine H. Grossman, Andrey A. Bobko, Margaret F. Bennewitz

Thermal decomposition of Mn(II) ACAC was performed in oleylamine and dibenzyl ether at two temperature ramp rates and increasing aging times at 300°C to form MnO NPs coated with oleylamine.

History

Licence

Exports