Modulation of Dark Conductivity over a 1 × 10−12 to 1 × 10−5 S/cm Range Through Ancillary Group Modification in Amorphous Solids of Ethyne-Bridged (Porphinato)zinc(II) Oligomers

Modulation of Dark Conductivity over a 1 × 10−12 to 1 × 10−5 S/cm Range Through Ancillary Group Modification in Amorphous Solids of Ethyne-Bridged (Porphinato)zinc(II) Oligomers